DNV A32 D32 E32 F32 Steel Plate

DNV Grades NV A32, NV D32, and NV E32 are high-strength structural steels with a minimum specified yield strength of 46 ksi and specified minimum Charpy V-notch impact toughness properties. DNV A32, D32, E32, and F32 are high-strength structural steel plates primarily used in shipbuilding and offshore construction due to their good toughness, high strength, and strong corrosion resistance. 

DNV A32 D32 E32 F32 Steel Plate Supplier

DNV Grades NV A32, NV D32, and NV E32 are high-strength structural steels with a minimum specified yield strength of 46 ksi and specified minimum Charpy V-notch impact toughness properties. DNV A32, D32, E32, and F32 are high-strength structural steel plates primarily used in shipbuilding and offshore construction due to their good toughness, high strength, and strong corrosion resistance.

These grades are part of the DNV (Det Norske Veritas) classification society standards for certified materials in the maritime industry. The key differentiator among them is the specified minimum Charpy V-notch impact test temperature. 
  • DNV A32: Impact test at 0°C.
  • DNV D32: Impact test at -20°C.
  • DNV E32: Impact test at -40°C.
  • DNV F32: Impact test at -60°C.

Applications

Typical applications include shipbuilding and mobile offshore drilling units and structures.

Specification Parameters
Basic Information

NV A32 D32 E32 Mechanical Properties

Tensile testing is performed in the transverse direction.

Grade
Thickness
(in)
Yield strength
(min ksi)
Tensile strength
(ksi)
Elongation A5 1)
(min %)
NV A32
0.1969 – 5.91
46
64 – 82
22
NV D32
0.1969 – 5.91
46
64 – 82
22
NV E32
0.1969 – 5.91
46
64 – 82
22

1) See DNV Rules for elongation requirements for alternative tensile specimens.

 

NV A32 D32 E32 Impact Properties

Grade
Thickness
(in)
Test temperature(°F)
Min Longitudinal Average Energy 1)
(ft-lbs)
NV A32
0.1969 – 2.00
32
23
NV A32
2.01 – 2.75
32
28
NV A32
2.76 – 5.91
32
34
NV D32
0.1969 – 2.00
-4
23
NV D32
2.01 – 2.75
-4
28
NV D32
2.76 – 5.91
-4
34
NV E32
0.1969 – 2.00
-40
23
NV E32
2.01 – 2.75
-40
28
NV E32
2.76 – 5.91
-40
34

1) Tests are to be taken in the longitudinal direction. Normally, transverse test specimens are not required unless otherwise specified in the order. Impact tests not required when material thickness is less than 0.236 in. unless otherwise specified.

No more than one value below the specified miniminum average energy but no less than 70% of the specfied minimum average energy value.

Minimum average energy for full-size specimens. Refer to DNV Rules for sub-size specimen energy requirements.

Service Support
DNV A32 D32 E32 F32 Steel Plate

DNV Steel Plate Grade Supplier

General Strength

NV A

NV B

NV D

NV E

High Strength

NV A32

NV D32

NV E32

NV F32

NV A36

NV D36

NV E36

NV F36

NV A40

NV D40

NV E40

NV F40

Extra Strength

NV A420

NV D420

NV E420

NV F420

NV A460

NV D460

NV E460

NV F460

NV A500

NV D500

NV E500

NV F500

NV A550

NV D550

NV E550

NV F550

NV A620

NV D620

NV E620

NV F620

NV A690

NV D690

NV E690

NV F690