Steel Standard:ABS (American Bureau of Shipping)

Rolling Type:Shipbuilding steel plate,High tension ship plate

Thickness:3mm-250mm

Width:1200mm-4200mm

Length:3000mm-18000mm

Heat Treatment:TMCP/Normalised

What is ABS AH32 Shipbuilding Steel Plate?

As a hot-rolled high tensile strength steel, AH32 is designed to resist the harsh saline conditions of marine environments, and micro-alloying technology is employed to enhance toughness and resistance to corrosion. As one of the highest performance steels produced in the world, the H series of shipbuilding steels is designed to excel in many mechanical properties.

Grade A steel is the impact force subjected to normal temperature (20 ° C).

Grade B steel impact force at 0 °C.

Grade D steel impact force at -20 °C.

Grade E steel impact force at -40 °C.

 

Equivalent steel grade of ABS AH32

Equivalent steel grade of ABS AH32

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV AH32

GL-A32

LR/AH32

BV/AH32

CCS/A32

K A32

R A32

RI/A32

Specification Parameters
Basic Information

ABS AH32 high Strength Chemical Composition

ABS AH32 high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

ABS AH32

0.18

0.1-0.50

0.90-1.6

0.035

0.035

0.015

Nb

V

Ti

Cu

Cr

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.2

0.4

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

ABS AH32 high strength property

ABS AH32 high strength property

Grade

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

ABS AH32

mm

Min Mpa

Mpa

Min  %

0

J

J

t≤50

315

440-590

22%

22

31

50<t≤70

315

440-590

22%

26

38

70<t≤100

315

440-590

22%

31

46

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal